Most people know that the mold temperature is too high to cause shrinkage problems, and usually prefer to lower the mold temperature to solve the problem. But sometimes if the mold
Jan 06, 2022
The product diagram of the shielding cover is shown in Figure 1. The maximum size of the product is ø85.7 mm x 55.20 mm, the average thickness of the plastic part is 1.50 mm, the m
Mar 10, 2021
How to avoid the flush of PC product?The flushing at the nozzle is generally due to the decomposition of the raw material and the generation of gas due to the shearing and overheat
Jul 14, 2020
Jan 15, 2020
when we get a inquiry info then we will send the quotation within two days. during this time we will calutae the mold price. total 7 steps.see details.
Jan 14, 2020
Jan 13, 2020
Some moldflow or molded products shows the welding lines or welding marks. how to avoid it? see the details below.